產(chǎn)品中心
PRODUCT
油氣集輸緩蝕劑
一、產(chǎn)品概述
本產(chǎn)品是以多種咪唑啉衍生物及咪唑啉-氨基酸衍生物復(fù)配而成,成膜性能優(yōu)異,緩蝕率高;抗分解性能強(qiáng),使用量低。不含金屬及其它對(duì)催化劑有害物質(zhì),對(duì)下游產(chǎn)品和加工過(guò)程無(wú)影響。復(fù)配構(gòu)成的液體緩蝕劑,具有緩蝕率高、凝固點(diǎn)低、分散性好、熱穩(wěn)定性好、低毒等優(yōu)點(diǎn),可迅速在金屬表面形成致密牢固的保護(hù)膜,對(duì)多種腐蝕因素都有較強(qiáng)緩蝕性能。本產(chǎn)品與其它井下用劑具有良好的配伍性。
本產(chǎn)品在國(guó)內(nèi)各大油田廣泛使用,本產(chǎn)品出口至中東以及南亞、南美等地區(qū)。
二、技術(shù)指標(biāo)
項(xiàng)目 |
檢測(cè)指標(biāo) |
外觀 |
黃色至紅棕色液體 |
密度(20℃,g/cm3) |
≥0.90 |
pH值 |
8.5-9.5 |
緩蝕率(%) |
≥90 |
腐蝕速率(g / (m2·h)) |
≤0.076 |
三、使用方法
Ⅰ、本產(chǎn)品首次使用時(shí),應(yīng)先預(yù)膜,加注可采用連續(xù)和間歇兩種方式。對(duì)于含硫生產(chǎn)氣井(無(wú)分隔器)建議由套管環(huán)空加注,經(jīng)油管返出形成一定循環(huán)體系;對(duì)于常關(guān)氣井建議分別從油、套管加入;對(duì)于油氣集輸管線可直接加注。
Ⅱ、預(yù)膜用量計(jì)算方法:
1、預(yù)膜面積:按氣井油管內(nèi)、外表面積+套管內(nèi)表面積+擬保護(hù)地面管線內(nèi)表面積;
2、預(yù)膜厚度:75μm。
Ⅲ、氣井建議周期性間歇加注,推薦加藥周期為30天,每次加量為80㎏。
油井建議連續(xù)性加藥,推薦用量:按產(chǎn)出液計(jì)算,推薦使用濃度200ppm。
四、包裝、運(yùn)輸與貯存
包裝:200L塑料桶包裝,凈重200±1kg。
運(yùn)輸:防日曬、雨淋,應(yīng)避免與腐蝕性物品和尖狀物品混運(yùn)。
貯存:置于干燥、通風(fēng)庫(kù)房,避免與腐蝕性的物品混放,保質(zhì)期1年。
五、安全與防護(hù)
皮膚與眼睛接觸:立即用大量清水沖洗。
誤食:飲足量溫水,催吐,就醫(yī)。
操作保護(hù):戴PVC、PE或橡膠手套。
泄漏:用大量清水沖洗。
Oil and Gas Pipeline Transmission System
Corrosion Inhibitor
Product Overview
In the oil and gas well produced fluid CO2 and H2S、CI - corrosive medium, such as content is higher, causing serious corrosion of casing, tubing.This product is imidazoline quaternary ammonium salt derivatives, double imidazoline, aldehyde, ketone condensation product of amine and other components of the corrosion and other auxiliary components distribution of liquid in the composition of the corrosion inhibitor. This product has the advantages of high corrosion inhibition rate, low freezing point, good dispersion, good thermal stability, low toxicity and so on. This corrosion inhibitor can quickly form a tight and firm protective film on the metal surface, and has a strong corrosion inhibition performance against a variety of corrosion factors.
This product has good compatibility with other downhole agents.
Technical indicators
Items |
Index |
appearance |
Yellow to reddish brown liquid |
density(20℃,g/cm3) |
≥0.90 |
pH |
8.5-9.5 |
inhibition rate (%) |
≥90 |
corrosion rate(g / (m2·h)) |
≤0.076 |
Methods used
Ⅰ、 When the product is first used, the film should be prefabricated. Continuous and intermittent injection can be used. For sulfur-bearing production gas Wells (without separators), it is suggested to refill by casing annulus and return through tubing to form a certain circulation system. It is suggested to add oil and casing respectively to the normally closed gas well.For oil and gas collection and transportation pipelines can be directly injected.
Ⅱ、Calculation method of prefilm dosage:
1. Pre-film area: the sum of the internal and external area of gas well tubing, the surface area of casing and the surface area of the pipeline to be protected;
2. Thickness of prefilm: 75 microns.
3. Gas well recommended periodic intermittent filling, recommended dosing period of 30 days, added amount 80 ㎏ each time.
Continuous dosing is recommended for oil Wells. Recommended dosage: calculated according to the output fluid, the recommended concentration is 200ppm.
Packing, Transportation 、Storage
Packing: 200L plastic drum, net weight 200kg.
ransportation: avoid sunburn and rain. Avoid mixed transportation with corrosive and sharp articles.
Storage: store in dry and ventilated warehouse, avoid mixing with corrosive materials, with a shelf life of 1 year.
Safety & amp; protection
Skin to eye contact: rinse immediately with plenty of water.
Ingestion: drink enough warm water, induce vomiting, seek medical advice.
Peration protection: wear PVC, PE or rubber gloves.